It uses cotton canvas,nylon canvas and polyester canvas as belt core, Hence, the belt body enjoys good elasticity, excellent grooving forming ability and small tensile rate.
The covering layer is processed with acid and alkaline resistance materials. Therefore, it is characterized by excellent chemical corrosion resistance performance and good physical performance.
MOR³ | DIN 22102 G | 15 | 450 | 200 | 1.12 | MBR/ SBR- |
60±5 | -30 până la +60 | Moderatelt oil resistant. Suitable for materials consisting of animal fat or vegetable oil. Sweling in ASTM 3oil (24 h, 1009C)max. +65% . |
PAS | MF/H-6* | 15 | 450 | 200 | 1.11 | MBR/ /BR/IR |
55±5 | -60 până la +60 | Suitable for materals consisting of pitch and turpentine. In result of ageing timp de 24 de ore la 20°C în ulei de terebentină modificarea volumului este de max.+45%. Poate fi operat la temperatura continua scazuta chiar si -60°C. Tip R conform DIN 22 102 Umflare în ulei ASTM 3 (24h, 100°C) max. +/-10%. |
SAU | DIN 22102 G | 12 | 300 | 200 | 1.25 | MBR | 60±5 | -20 până la +100 | High degree resistance aginst mineral oils. Suitable for materials constând |