It uses cotton canvas,nylon canvas and polyester canvas as belt core, Hence, the belt body enjoys good elasticity, excellent grooving forming ability and small tensile rate.
The covering layer is processed with acid and alkaline resistance materials. Therefore, it is characterized by excellent chemical corrosion resistance performance and good physical performance.
MOR³ | DIN 22102 G | 15 | 450 | 200 | 1.12 | MBR/ SBR- |
60±5 | -30 ilə +60 arasında | Moderatelt oil resistant. Suitable for materials consisting of animal fat or vegetable oil. Sweling in ASTM 3oil (24 h, 1009C)max. +65% . |
PITCH | MF/H-6* | 15 | 450 | 200 | 1.11 | MBR/ /BR/IR |
55±5 | -60 ilə +60 arasında | Suitable for materals consisting of pitch and turpentine. In result of ageing 20°C-də 24 saat ərzində skipidar yağında həcm dəyişikliyi maks.+45% təşkil edir. Davamlı aşağı temperaturda hətta -60°C-də işləyə bilər. DIN 22 102 uyğun olaraq R növü ASTM 3 yağında şişmə (24 saat, 100°C) max. +/-10%. |
YA | DIN 22102 G | 12 | 300 | 200 | 1.25 | MBR | 60±5 | -20 ilə +100 arasında | High degree resistance aginst mineral oils. Suitable for materials ibarət |